ORIGINAL ARTICLE
Year : 2022  |  Volume : 11  |  Issue : 1  |  Page : 51

Orthodontic bond strength with the use of non-aerosol producing bonding primers in lieu of conventional primers: An in vitro evaluation


Department of Orthodontics and Dentofacial Orthopaedics, I.T.S. Center for Dental Studies and Research, Muradnagar, Ghaziabad, Uttar Pradesh, India

Correspondence Address:
Monis Raza
Senior Lecturer, Department of Orthodontics and Dentofacial Orthopaedics, I.T.S. Center for Dental Studies and Research, Muradnagar, Ghaziabad, Uttar Pradesh - 201 206
India
Login to access the Email id

Source of Support: None, Conflict of Interest: None


DOI: 10.4103/jos.jos_134_21

Rights and Permissions

OBJECTIVE: To evaluate the efficacy of non-aerosol producing restorative self-etching primers (SEPs) as a substitute for conventional orthodontic bonding primers and to analyze the extent of residual composite on the tooth post-debonding. MATERIALS AND METHODS: Eighty-four extracted human premolars were randomly divided into seven groups based on the adhesive and the bonding protocol used. The study comprised Prime and Bond one select (Dentsply), G-Premio Bond (GC), which were each divided into three subgroups based on the method used for moisture control and the control group (Transbond XT conventional total etch). The three methods for moisture control in study groups were: without drying, air-drying with the use of a three-way syringe, and with the use of blotting paper. Shear bond strength (SBS) was tested using a universal testing machine (UTM), and after debonding, the enamel surface of each tooth was examined under 10× magnification to evaluate adhesive remaining index (ARI) scores. RESULTS: Groups 2A (Prime and Bond; without drying) & 1 (Transbond XT) had the lowest and highest SBS values, respectively (P = 0.001). Comparison of ARI between the control group and group 2b (Prime and Bond; air-drying with 3 in 1) showed a significant difference (P = 0.041). Comparison of ARI between control group and group 2c (Prime and Bond; blotting paper) showed a significant difference (P = 0.017). Rest all other comparisons were non-significant. CONCLUSIONS: Transbond XT had SBS values higher than the self-etch groups. Among the self-etch groups, G-Premio Bond had higher SBS values when the traditional methods of air-drying were followed. Use of blotting paper for drying that produced variable SBS values can be an effective alternative method. G-Premio Bond with its adequate bond strength under manufacturer's instruction seems promising in this regard.


[FULL TEXT] [PDF]*
Print this article     Email this article
 Next article
 Previous article
 Table of Contents

 Similar in PUBMED
   Search Pubmed for
   Search in Google Scholar for
 Related articles
 Citation Manager
 Access Statistics
 Reader Comments
 Email Alert *
 Add to My List *
 * Requires registration (Free)
 

 Article Access Statistics
    Viewed1448    
    Printed94    
    Emailed0    
    PDF Downloaded156    
    Comments [Add]    

Recommend this journal